Thermal relaxation of lithium dendrites
Asghar Aryanfar, Daniel J. Brooks, Agustín J. Colussi, Boris V. Merinov, William A. Goddard III, Michael R. Hoffmann
Abstract
The average lengths λ^- of lithium dendrites produced by charging symmetric Li^0 batteries at various temperatures are matched by Monte Carlo computations dealing both with Li^+ transport in the electrolyte and thermal relaxation of Li0 electrodeposits. We found that experimental λ^-(T) variations cannot be solely accounted by the temperature dependence of Li^+ mobility in the solvent but require the involvement of competitive Li-atom transport from metastable dendrite tips to smoother domains over ΔE^(‡)_R ~ 20 kJ mol^−1 barriers. A transition state theory analysis of Li-atom diffusion in solids yields a negative entropy of activation for the relaxation process: ΔS^(‡)_R ≈ −46 J mol^−1 K^−1 that is consistent with the transformation of amorphous into crystalline Li0 electrodeposits. Significantly, our ΔE^(‡)R ~ 20 kJ mol^−1 value compares favorably with the activation barriers recently derived from DFT calculations for self-diffusion on Li^0(001) and (111) crystal surfaces. Our findings suggest a key role for the mobility of interfacial Li-atoms in determining the morphology of dendrites at temperatures above the onset of surface reconstruction: TSR ≈ 0.65 T_MB (T_MB = 453 K: the melting point of bulk Li^0).
Group Members
Aryanfar, A., Brooks, D. J., Colussi, A. J., Merinov, B. V., III, W. A. G., & Hoffmann, M. R. (2015). Thermal relaxation of lithium dendrites. *Phys. Chem. Chem. Phys.*, *17*(12), 8000-8005. https://doi.org/10.1039/c4cp05786d